Degussa AG Trogamid® CX9710 Transparent Nylon
  Subcategory: Nylon; Thermoplastic 
Key Words: PA PACM 12, cycloaliphatic diamine dodecanedioic acid 
Material Notes:  Description: TROGAMID® CX compounds round off the product range of High Performance Polymers to include semicrystalline polyamides, the crystallites of which are so small that they do not scatter visible light—a property known as microcrystallinity. The compounds are therefore as clear as glass. They possess higher resistance to chemicals and stress cracking than amorphous transparent plastics, in addition to the mechanical advantages of amorphous compounds. The outstanding properties of TROGAMID® CX are:- crystal-clear, permanent transparency; high transmission
 - superior chemical and stress cracking resistance
 - high level of UV resistance
 - low water absorption, which leaves the mechanical properties virtually unaffected
 - high dimensional stability
 - balanced mechanical property profile
 - high impact resistance, even at low temperatures
 - high level of dynamic strength (e.g., for internally pressurized parts)
 - abrasion and scratch resistance
 - high glass transition temperature
 - very low isotropic shrinkage
 - easy processing
 
  The unique combination of properties in TROGAMID® CX compounds permits their use over a broad application spectrum. Areas of application can be as diverse as water management, filter technology, laboratory and medical technology, the manufacture of eyeglasses, or bottles for the cosmetics industry. Specific Notes for this Material: Medium-viscous, permanently transparent polyamide for injection molding and extrusion, with an internal mold release agent Information provided by degussa. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Melt Density
 
- Viscosity Test
 
- Hardness, Shore D
 
- Ball Indentation Hardness
 
- Tensile Strength at Break
 
- Tensile Strength, Yield
 
- Elongation at Break
 
- Elongation at Yield
 
- Tensile Modulus
 
- Flexural Modulus
 
- Flexural Strength
 
- Charpy Impact Unnotched
 
- Charpy Impact, Notched, Low Temp
 
- Charpy Impact, Unnotched Low Temp
 
- Charpy Impact, Notched
 
- Volume Resistivity
 
- Surface Resistance
 
- Dielectric Constant, Low Frequency
 
- Dissipation Factor
 
- Dissipation Factor, Low Frequency
 
- Comparative Tracking Index
 
- CTE, linear 20°C
 
- Specific Heat Capacity
 
- Thermal Conductivity
 
- Melting Point
 
- Maximum Service Temperature, Air
 
- Deflection Temperature at 0.46 MPa (66 psi)
 
- Deflection Temperature at 1.8 MPa (264 psi)
 
- Vicat Softening Point
 
- Glass Temperature
 
- Flammability, UL94
 
- Glow Wire Test
 
- Carreau-WLF K1
 
- Carreau-WLF K2
 
- Carreau-WLF K3
 
- Carreau-WLF K4
 
- Carreau-WLF K5
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |