Degussa AG Trogamid® CX9710 Transparent Nylon

 

Subcategory: Nylon; Thermoplastic

Key Words: PA PACM 12, cycloaliphatic diamine dodecanedioic acid

Material Notes:
Description: TROGAMID® CX compounds round off the product range of High Performance Polymers to include semicrystalline polyamides, the crystallites of which are so small that they do not scatter visible light—a property known as microcrystallinity. The compounds are therefore as clear as glass. They possess higher resistance to chemicals and stress cracking than amorphous transparent plastics, in addition to the mechanical advantages of amorphous compounds. The outstanding properties of TROGAMID® CX are:

  • crystal-clear, permanent transparency; high transmission
  • superior chemical and stress cracking resistance
  • high level of UV resistance
  • low water absorption, which leaves the mechanical properties virtually unaffected
  • high dimensional stability
  • balanced mechanical property profile
  • high impact resistance, even at low temperatures
  • high level of dynamic strength (e.g., for internally pressurized parts)
  • abrasion and scratch resistance
  • high glass transition temperature
  • very low isotropic shrinkage
  • easy processing

The unique combination of properties in TROGAMID® CX compounds permits their use over a broad application spectrum. Areas of application can be as diverse as water management, filter technology, laboratory and medical technology, the manufacture of eyeglasses, or bottles for the cosmetics industry.

Specific Notes for this Material: Medium-viscous, permanently transparent polyamide for injection molding and extrusion, with an internal mold release agent

Information provided by degussa.

Available Properties
  • Density
  • Melt Density
  • Viscosity Test
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant, Low Frequency
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Flammability, UL94
  • Glow Wire Test
  • Carreau-WLF K1
  • Carreau-WLF K2
  • Carreau-WLF K3
  • Carreau-WLF K4
  • Carreau-WLF K5
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。