Degussa AG Trogamid® T5000 Nylon 6-3

 

Subcategory: Nylon; Thermoplastic; Nylon 6-3

Key Words: PA 6-3-T, PA NDT/INDT, trimethyl hexamethylene diamine terephthalic acid

Material Notes:
Description: TROGAMID® T compounds are distinguished by the following properties:

  • crystal-clear, optical transparency
  • high mechanical stability
  • high thermostability
  • high viscosity
  • good chemical resistance compared to other plastics
  • good electrical properties
  • low mold shrinkage

The special properties of TROGAMID T have made it useful in many branches of industry:

  • Electrical Industry:
    • high-voltage switch casings
    • cable glands
    • battery seals
    • keys and push buttons
    • terminal strips
    • casings for switches, relays, and counters
    • gearwheels and gear racks
  • Water Resource Management and Filter Technology:
    • filter cups for pneumatic systems
    • filter cups for water treatment
    • fuel filter cups
    • pump casings
    • metering devices
    • inspection glasses
  • Machine and Apparatus Construction:
    • flowmeters
    • liquid-level indicators
    • valve blocks and common control blocks for dispensing and metering equipment
    • guide rails

Specific Notes for this Material: Permanently transparent polyamide for injection molding, extrusion, and blow molding; no additives

Information provided by degussa.

Available Properties
  • Density
  • Viscosity Test
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1000 hours
  • Abrasion
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Glass Temperature
  • UL RTI, Mechanical with Impact
  • UL RTI, Mechanical without Impact
  • Flammability, UL94
  • Glow Wire Test
  • Color
  • Scratch Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。