Degussa AG Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Subcategory: Nylon; Thermoplastic; Polymer
Key Words: PA 6-3-T, PA NDT/INDT, trimethyl hexamethylene diamine terephthalic acid
Material Notes: Description: TROGAMID® T compounds are distinguished by the following properties:- crystal-clear, optical transparency
- high mechanical stability
- high thermostability
- high viscosity
- good chemical resistance compared to other plastics
- good electrical properties
- low mold shrinkage
The special properties of TROGAMID T have made it useful in many branches of industry: - Electrical Industry:
- high-voltage switch casings
- cable glands
- battery seals
- keys and push buttons
- terminal strips
- casings for switches, relays, and counters
- gearwheels and gear racks
- Water Resource Management and Filter Technology:
- filter cups for pneumatic systems
- filter cups for water treatment
- fuel filter cups
- pump casings
- metering devices
- inspection glasses
- Machine and Apparatus Construction:
- flowmeters
- liquid-level indicators
- valve blocks and common control blocks for dispensing and metering equipment
- guide rails
Specific Notes for this Material: Amorphous polyamide, 35% glass fiber reinforced, for the injection molding of stiff, low-warpage moldings; can be mixed with TROGAMID T5000 to form compounds with a low glass fiber content whose general properties can be adjusted to fit a particular application. Information provided by degussa.
| Available Properties |
- Density
- Viscosity Test
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|