|   Degussa AG VESTAMID® L1640 nf (as-conditioned) Nylon 12  Subcategory: Nylon; Thermoplastic; Nylon 12 Close Analogs: This former Creanova product line is a part of Degussa AG  as of 2001. This grade  is not part of the current Degussa product line. Key Words: Polyamide Material Notes: ISO data as provided by the manufacturer, Creanova, Inc.
 Uses: Wire insulation, fiber optics jacketing. 
| | 
    | Available Properties |  
    | DensityMoisture Absorption at EquilibriumTensile Strength, YieldElongation at BreakElongation at YieldModulus of ElasticityCharpy Impact UnnotchedCharpy Impact, Notched, Low TempCharpy Impact, Unnotched Low TempCharpy Impact, NotchedElectrical ResistivitySurface ResistanceDielectric ConstantDielectric Constant, Low FrequencyDielectric StrengthDissipation FactorDissipation Factor, Low FrequencyCTE, linear 20°CDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Vicat Softening PointUL RTI, ElectricalUL RTI, Mechanical with ImpactUL RTI, Mechanical without Impact
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |