Degussa AG Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 612; Polymer
Key Words: PA612-HI, MH, 14-040, GF10
Material Notes: Description: impact-resistant, 10% glass fiber reinforced, medium-viscosity, heat-stabilized Applications: housings subject to impact, coverings with molded-on elastomer seals Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|