|   Degussa AG Vestamid® DX9321 Black 20% Glass Reinforced Nylon 612 (Conditioned)  Subcategory: Nylon; Thermoplastic; Nylon 612; Polymer Key Words: PA612-HI, MH, 14-050, GF20 Material Notes: Description: impact-resistant,20% glass fiber reinforced, heat-stabilized
 Applications: housings, coverings Information provided by degussa. 
| | 
    | Available Properties |  
    | DensityTensile Strength at BreakTensile Strength, YieldElongation at BreakElongation at YieldTensile ModulusCharpy Impact UnnotchedCharpy Impact, Notched, Low TempCharpy Impact, Unnotched Low TempCharpy Impact, NotchedMelting PointDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Vicat Softening PointFlammability, UL94
 | 
 | 
 |  | | 