Degussa AG Vestamid® E40-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer

 

Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Nylon; Thermoplastic; Nylon 12

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: noiseless gears, seals, functional elements of sports shoes, process aids in the extrusion of thermoplastic polyurethanes, films

Information provided by degussa.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Viscosity Test
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • 50% Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Tensile Creep Modulus, 1000 hours
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。