Degussa AG Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Nylon; Thermoplastic; Nylon 12
Material Notes: Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:- They have low density.
- They are highly resistant to chemicals and solvents.
- They are easy to process and color and are easy to overmold.
- They can be decorated easily by means of heat transfer printing.
- They have excellent impact strength at low temperatures.
- Their hardness and flexibility can be varied over a wide range.
- They have high elasticity and good recovery.
- Their mechanical properties are only slightly temperature-dependent.
- They are free of volatile or migrating plasticizers.
Applications: alpine ski boots, noiseless gears, conveyor belts Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Viscosity Test
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- 50% Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1000 hours
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|