|   Degussa AG Vestamid® L2106F Nylon 12  Subcategory: Nylon; Thermoplastic; Nylon 12 Material Notes: Description: High-viscosity film grade, improved transparency, modified by co-monomers
 Applications: Flexible tubular film for sausage casings Information provided by degussa. 
| | 
    | Available Properties |  
    | DensityMoisture Absorption at EquilibriumWater Absorption at SaturationLinear Mold ShrinkageLinear Mold Shrinkage, TransverseTensile Strength, YieldElongation at BreakElongation at YieldTensile ModulusCharpy Impact UnnotchedCharpy Impact, Notched, Low TempCharpy Impact, Unnotched Low TempCharpy Impact, NotchedVolume ResistivityDielectric ConstantDielectric Constant, Low FrequencyDielectric StrengthDissipation FactorDissipation Factor, Low FrequencyComparative Tracking IndexCTE, linear 20°CMelting PointDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Vicat Softening PointFlammability, UL94Electrolytic Corrosion
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |