Degussa AG Vestamid® L-R3-EP Antistatic, Black, Electrically Conductive Nylon 12

 

Subcategory: Nylon; Thermoplastic; Nylon 12

Key Words: PA12-P,EHZ,22-007

Material Notes:
Description: High-viscosity, plasticized, heat- and light-stabilized

Applications: Antistatic and electrically conductive moldings or extrudates for use in areas prone to explosions such as coal mining and other industries; e.g., housings for explosion-protected measuring equipment or for electric switches, ventilation fans for electric motors, chair castors, loudspeaker boxes, telephone and radio equipment, profiles for guide rails in assembly lines in the electronics industry. Also with electric shock protection.

Information provided by degussa.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Volume Resistivity
  • Insulation Resistance
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。