Degussa AG Vestamid® X7163 High Viscosity, Heat Stabilized, Graphite Filled Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: VESTAMID X7163 black is a graphite-filled and heat-stabilized compound for extrusion. Its improved properties of sliding friction make it most suitable for the production of push-pull cable liners. Further advantages of VESTAMID X7163black are the characteristic properties of PA 12like small water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity. Information provided by degussa.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|