Degussa AG Vestamid® X7293 Plasticized Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Key Words: PA12-HIP, EHL,22-004
Material Notes: Description: High-viscosity, plasticized, heat- and light-stabilized, with processing aid, increased low-temperature impact strength Applications: Fuel, vacuum and hydraulic lines; tubing for air brake lines, meets DIN 73378, 74324, ISO 7628, SAE J844 Information provided by degussa.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|