Degussa AG Vestamid® X7380 23% Glass, Antistatic, Black, Electrically Conductive Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Key Words: PA12-HI,MHZ,16-050,GF23
Material Notes: Description: Medium-viscosity,23% chopped strands, heat- and light-stabilized, increased impact strength Applications: Quick connectors in conductive fuel lines Information provided by degussa.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Insulation Resistance
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|