Degussa AG Vestamid® LX9104 Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: VESTAMID LX9104 is a halogen-free flame-retardant and flexible PA 12 compound of flammability class V-0 at0.8mm according to UL 94 and a LOI of 28%. Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
|
|
|
|