Creanova VESTOLIT® Pulver 5401 PVC-HI
Subcategory: Vinyl; Thermoplastic
Key Words: Polyvinyl Chloride; Creanova Inc. (Huls)
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Window sections for use in temperate central-European-like climate.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Tensile Impact Strength
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- CTE, linear 20°C
- Vicat Softening Point
|
|
|
|
| Property Data |