Degussa AG VESTORAN® X4890 sw PPE
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Impact resistant PPE resin with a heat deflection temperature of 125°C. VESTORAN X4890 has a very good flow properties and a high impact resistance. Parts with large surfaces exhibit a regular matte surface finish. Applications: Housing parts, automotive industry, electroindustry, environmental technology.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Impact Strength
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|