Degussa AG Vestodur® CL2030 30% Glass Reinforced, Crosslinkable PBT Based Compound
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: VESTODUR CL2030 is a 30 % glass fiber-reinforced, self-extinguishing compound for injection molding, based on modified polybutylene terephthalate (PBT).Moldings of VESTODUR CL2030 can be crosslinked by high-energy radiation (ß- or ?-radiation) or heat. The influence of the radiation to the mechanical properties is negligible. The short-term heat resistance is increased up to 400 °C depending on the conditions. Crosslinked parts of VESTODUR CL2030 can be used in common soldering processes like surge soldering, vapor phase soldering or IR soldering which are typical in the electronic industry. The incorporated flame retardant is non-migrating and has no corrosive effects on metal inserts or neighboring metal parts. Laser marking with high contrast is possible. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|