Degussa AG Vestodur® CL2130 30% Glass Reinforced, Crosslinkable PBT Based Compound

 

Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer

Material Notes:
Description: VESTODUR CL2130 is a 30 % glass fiber reinforced, self-extinguishing compound for injection molding, based on modified polybutylene terephthalate (PBT).Moldings of VESTODUR CL2130 can be crosslinked by high-energy radiation (ß- or ?-radiation) or heat. The influence of the radiation to the mechanical properties is negligible. The short-term heat resistance is increased up to 350°C depending on the conditions. Crosslinked parts of VESTODUR CL2130 can be used in common soldering processes like surge soldering, vapor phase soldering, and IR soldering which are typical in the electronic industry. The incorporated flame retardant is non-migrating and has no corrosive effects on metal inserts or neighboring metal parts. Due to a special additive this PBT compound can be metallized selectively.

Information provided by degussa.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。