Degussa AG Vestodur® RS 1404 12% Glass Reinforced, Radiation Crosslinkable PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:- high thermostability
- high stiffness
- low water absorption resulting in high dimensional stability
- high hardness
- good strength
- good sliding friction behavior, low abrasion
- good creep behavior
- good electrical properties
- good chemical resistance
- good weathering resistance
- good processability
- no tendency to form stress cracks
Specific Notes for this Material: Crosslinkable with heat (180-200°C, 5-12 hr), with flame retardant Information provided by degussa.
| Available Properties |
- Melt Flow
- Tensile Modulus
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|