Degussa AG Vestodur® X7085 45% Glass Fiber Reinforced PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Description: VESTODUR X7085 is a 45 % glass fiber-reinforced, polymer-modified polybutylene terephthalate compound for injection molding. The compound is suitable for parts that are subjected to high mechanical and thermal loads. Compared with commonly used glass fiber-reinforced PBT compounds with similar stiffness parts of VESTODUR X7085 have in particular a high surface quality. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|