Degussa AG Vestodur® X7285 30% Glass Fiber Reinforced PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Description: VESTODUR X7285 is a 30% glass fiber reinforced compound based on polymer-modified polybutylene terephthalate (PBT) for injection molding. The compound is suitable for parts with high mechanical and thermal resistance. In contrast to common glass fiber reinforced PBT compounds with comparable stiffness moldings of VESTODUR X7285 show in particular a high surface quality. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|