Degussa AG Vestodur® X7390 Heat Stabilized PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Description: VESTODUR X7190 and X7390 are unreinforced, heat-stabilized and polymer modified polybutylene terephthalate (PBT) compounds with low shrinkage for extrusion. The compounds are especially suitable for the manufacture of stiff, small diameter tubing, e.g., loose buffering for fiber optics. VESTODUR X7390 has increased hydrolysis and heat resistance. Compared with standard PBT compounds X7190 and X7390 are harder. Therefore, they can also be used to protect as outer sheaths to protect electrical cables from the chewing of rodents. Both compounds contain a processing aid which facilitates feeding in the extrusion process. Information provided by degussa.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|