Degussa AG Vestodur® X9400 10% Glass Reinforced PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: VESTODUR X9400 is a 10 % glass fiber reinforced, polymer-modified polybutylene terephthalate compound. Moldings of this compound show decreased shrinkage. The compound is suitable for parts that are subjected to high mechanical or thermal loads. Compared with commonly used glass fiber reinforced PBT compounds with a similar stiffness parts of VESTODUR X9400 have in particular a high surface quality Information provided by degussa.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|