Degussa AG Vestoran® RD 3530 SBR Rubber/Plastic Composite
Subcategory: Styrene-Butadiene; Thermoplastic
Material Notes:
Formulation| SBR 1500 | 100 | | Carbon Black N 550 | 50 | | Paraffin Oil | 5 | | ZnO | 3 | | Stearic Acid | 1 | | Sulfur | 1.75 | | Vulkacit®NZ(TBBS) | 1 | Information provided by degussa.
| Available Properties |
- Viscosity Measurement
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 200% Modulus
- 300% Modulus
- Rebound
|
|
|
|