Degussa AG Vestoran® RD 3731 XNBR Rubber/Plastic Composite
Subcategory: Thermoplastic
Material Notes:
Formulation| Nipol® 1472 (or Chemigum® NX 775) | 100 | | Sillitin® Z 86 | 60 | | Polestar® 200 (Calc. Clay) | 20 | | Carbon Black N 660 | 3 | | Vulkanol® 88 | 10 | | Stearic Acid | 1 | | BDMA | 1.5 | | Perkadox® 14/40 | 6 | Information provided by degussa.
| Available Properties |
- Viscosity Measurement
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 200% Modulus
- Rebound
- Tear Strength
- Compression Set
|
|
|
|
| Property Data |