Degussa AG Vestoran® RD 5010 NR/SBR Rubber/Plastic Composite
Subcategory: Styrene-Butadiene; Thermoplastic
Material Notes:
Formulation| NR | 80 | | SBR 1500 | 20 | | Carbon Black N 772 | 59 | | ZnO | 4 | | Stearic Acid | 1 | | Vulkanox® HS(TMQ) | 1.2 | | Vulkanox®4020(IPPD) | 2 | | Antilux® 600 | 2 | | Sulfur | 4 | | Vulkacit® CZ(CBS) | 0.65 | | Vulkalent® E | 0.2 | Information provided by degussa.
| Available Properties |
- Viscosity Measurement
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 200% Modulus
- 300% Modulus
- Rebound
- Tear Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|