Degussa AG Vestoran® RD 5114 EPDM Rubber/Plastic Composite
Subcategory: Thermoplastic
Material Notes:
Formulation| BUNA® EP G 6470 | 90 | | VESTENAMER® 8012 | 10 | | Carbon Black N 539 | 72 | | Paraffin Oil | 51 | | ZnO | 5 | | Vulkanox® HS (TMQ) | 1 | | TRIM | 1.25 | | Perkadox® 14/40 | 5.5 | Information provided by degussa.
| Available Properties |
- Density
- Viscosity Measurement
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Rebound
- Tear Strength
- Compression Set
|
|
|
|