Degussa AG Vestoran® X7342 20% Glass Reinforced Laser Markable PPE Compound
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Material Notes: Description: The polyphenylene ether compounds (PPE) VESTORAN® are amorphous materials with high heat deflection temperature. VESTORAN® compounds and the parts produced from them have the following properties:- very low water absorption
- hot water-resistant
- resistant to alkalis and acids
- very low mold shrinkage
- very low tendency to warp
VESTORAN® has proved to be highly suitable for production of coil bodies for vehicle electricity on account of its high dimensional stability, heat deflection temperature, dielectric strength, and ability to bond well to insulating compounds (epoxy resins). In addition, its low water absorption makes it a good choice for producing impellers for water pumps, for example, in engine cooling, but also for applications in machinery and engineering. Further applications include relay sockets, distributor cabinets, and large capacitor cases. Information provided by degussa.
| Available Properties |
- Tensile Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|