Huntsman PP 38S05A Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: High impact copolymer and FDA compliant. Features: Fractional melt flow and high impact. Applications: Extrusion: thermoformable sheet. FDA Notes: General purpose, limited FDA conformance. Information provided by Huntsman Corporation