Huntsman PP 23R2A Random Copolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliant Features: High contact clarity, non-blushing, toughness, impact, chemical, solvent, stress crack resistance, stiffness, hardness, heat resistance, exceptional high clarity and impact strength. Applications: Blow molded: radiation sterilizable vials and bottles. FDA Notes: 21 CFR 177.1520 (c)3.2; under conditions of use B through H described in 21 CFR 176.170 Table 2 Information provided by Huntsman Corporation
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|