Huntsman P9H2A-031 Impact Copolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Polypropylene, UL certified, and FDA compliant. Features: High impact and high blush resistance. Applications: Injection molding: furniture, outdoor application, and profile extrusion. Information provided by Huntsman Corporation
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Low Temperature Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|