Huntsman PE 1017 Film Extrusion Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer

Key Words: LDPE

Material Notes:
Homopolymer, Drug Master File listed product, and FDA compliant.

Features: Good impact strength, good machinability, heat seal and foaming characteristics

Applications: Film Extrusion: industrial liner/extrusion grade, drum liners, hardware packaging, furniture covers, and refuse bags.

FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170

Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.

Information provided by Huntsman Corporation

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Dart Drop
  • Dart Drop Test
  • Vicat Softening Point
  • Gloss
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。