Huntsman PE1061 Film Extrusion Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: LDPE
Material Notes: Homopolymer and FDA compliant. Features: Exceptional strength, good machinability and heat seal characteristics. Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink, and bundling. FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170 Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1. Information provided by Huntsman Corporation
| Available Properties |
- Density
- Thickness
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Secant Modulus, MD
- Secant Modulus, TD
- Dart Drop
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|