Huntsman PE1203 EVA Film Extrusion
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Key Words: Poly(Ethylene Vinyl Acetate)
Material Notes: 2% Vinyl Acetate EVA copolymer and FDA compliant Features: High clarity film with good stiffness and low temperature toughness. Applications: Film extrusion: food packaging, general purpose packaging that requires low temperature toughness. FDA Notes: Conforms to FDA regulation 21 CFR 177.1350 under condition of use C through G described in Table 2 of 21 CFR 176.170 Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1. Information provided by Huntsman Corporation
| Available Properties |
- Density
- Thickness
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Secant Modulus, MD
- Secant Modulus, TD
- Dart Drop
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|