Huntsman PE2049 Injection Molding Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE
Key Words: LDPE
Material Notes: Homopolymer, Drug Master File listed product, and FDA compliant. Features: Good molding processability, produces parts that are flexible, and show excellent flatness in large projected areas. Applications: Injection molding: general purpose molding, housewares, and industrial parts. FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170 Information provided by Huntsman Corporation
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|