Huntsman PE2051 Injection Molding Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE
Key Words: LDPE
Material Notes: Homopolymer and FDA compliant. Features: Very good molding processability, produces parts with good stiffness, and shows excellent flatness in large projected areas. Also recommended for multi-cavity, fast cycle products, and low melt temperature. Applications: Injection molding: housewares, industrial parts, and general purpose molding where improved gloss and stiffness is required. FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170 Information provided by Huntsman Corporation
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|