Huntsman Rexell® L8101 Cast Film Extrusion LLDPE
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Linear Low Density Polyethylene
Material Notes: Linear-low density copolymer, general purpose blown film extrusion, FDA compliant. Features: Excellent combination of sealability, mechanical strength and optics. Applications: Sealing layer in coextruded films principally for food packaging, heavy duty shipping sacks, and general purpose film FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2a. Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1. Information provided by Huntsman Corporation
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|