Hexcel Carbon Epoxy HexMC™ / C / 2000 / R1 Composite SMC
Subcategory: Epoxy; Composite SMC; Thermoset
Key Words: Hexcel Corporation; Carbon Fiber Composite Sheet Moilding Compound
Material Notes: High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications. Overall Features: - Competitive alternative to lightweight alloys (Ti, Al, Mg)
- Designed for compression molding
- Rapid processing cycles
- Complex shapes
- Molded-in inserts
- No material waste
- Internal release agent for multiple demolding
Provided as a 460 mm wide roll; 8 month shelf life at -18° C; 7 day shelf life at RT; Areal weight 2000 g/m²; 57% HS carbon fiber by volume; 2.5 min cure time per mm part thickness.Information provided by Hexcel Composites.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
- Shear Strength
- Glass Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|