ICOTEX™ 520-5004, 1000 Micron EVA Powder
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a vinyl acetate content of 28%. Information provided by ICO Polymers.
| Available Properties |
- Density
- Particle Size
- Vinyl Acetate Content
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Melting Point
- Max Dry Flow
|
|
|
|