ICORENE™ 115-1327, LMDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic
Material Notes: Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical properties. Key Characteristics: easy processing, good rigidity, good scratch resistance. Applications: This ICORENE® grade is particularly suitable for use in playground applications. Information provided by ICO Polymers.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact
- UV Light Weatherometer Test
|
|
|
|