ICORENE™ 324-3561, LMDPE Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic
Material Notes: Description: ICORENE 324-3561 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and melt out very quickly. Key Characteristics: fast molding, quick removal of surface pinholes, good balance of physical properties. Applications: This ICORENE® grade is particularly suitable for use in high flow applications. Information provided by ICO Polymers.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact
- UV Light Weatherometer Test
|
|
|
|