ICORENE™ 440-1312, PP Rotational Molding Resin
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: ICORENE 440-1312 is a polypropylene copolymer developed for rotational molding applications. The resin is fully UV protected. Key Characteristics: very high rigidity, good creep resistance, good high temperature resistance. Information provided by ICO Polymers.
| Available Properties |
- Density
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|