Idemitsu Xarec N WA 7010 SPS, 10% Glass Filled
Subcategory: Polystyrene; Thermoplastic; Syndiotactic Polystyrene; Polymer
Material Notes: Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|