Industrial Laminates/Norplex NP605 Paper Base Laminate
Subcategory: Phenolic; Thermoset
Key Words: Micarta
Material Notes: Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operation. However, it is also used in other industries for tooling stock because of its ease of machining and good dimensional stability. Thickness Tested: 0.062", 0.125" and 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Flexural Strength
- Compressive Strength
- Dielectric Breakdown
- Flammability, UL94
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|