Industrial Laminates/Norplex NP843 Paper Base Laminate
Subcategory: Phenolic; Thermoset
Key Words: Micarta
Material Notes: Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through and on the surfaces. Thickness Tested: 0.062", 0.125", and 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Unnotched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Flammability, UL94
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|