Industrial Laminates/Norplex MC320LE Cotton Fabric
Subcategory: Phenolic; Thermoset
Key Words: Micarta
Material Notes: Description: Grade MC320LE is a fine weave bleached cotton phenolic composite that has excellent machining characteristics and low moisture absorption. Applications include marine applications, terminal boards and parts requiring medium strength and excellent electrical characteristics. Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Unnotched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Breakdown
- Dissipation Factor
- Arc Resistance
- UL RTI, Electrical
- UL RTI, Mechanical without Impact
- Bond Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|