Industrial Laminates/Norplex NP511 Glass Fabric
Subcategory: Glass; Glass Fiber; Thermoset
Key Words: Micarta
Material Notes: Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Material meets or exceeds NEMA G-11 standard and has been produced using the same materials as listed in the NIST G11CR specification for materials used in cryogenic applications, but not to the exact same quantities of ingredients as specified in the process specification. Thickness Tested: 0.062", 0.125" & 0.500" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Unnotched
- Dielectric Constant
- Dielectric Strength
- Dielectric Breakdown
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Bond Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|