Industrial Laminates/Norplex NP524MG Glass Fabric
Subcategory: Glass; Glass Fiber; Thermoset
Key Words: Micarta
Material Notes: Description: NP524MG is made with a woven glass fabric in combination with high temperature, conductive epoxy resin system. NP524MG has excellent flexural, compressive and impact strengths at room temperature and elevated temperatures. It was developed for the motor generator industry to provide conductive coupling to eliminate static discharges caused by corona. It is capable of continuous operation exceeding 175°C. Thickness Tested: 0.062”, 0.125”, and 0.500” Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Flexural Modulus
- Flexural Strength
- Shear Strength
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Bond Strength
- Conductivity Range Surface
- Degradation Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|