Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Subcategory: Glass; Glass Fiber; Thermoset
Key Words: Micarta
Material Notes: Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined parts. Excellent mechanical strength at elevated temperatures. The continuous operating temperature is 190°C.Short excursions to temperatures approaching 360°C, such as in wave soldering or IR re-flow, will not adversely affect the life of this material. Thickness Tested: 0.062" & 0.315" Information provided by Industrial Laminates/Norplex.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell M
- Tensile Strength, Yield
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Unnotched
- Volume Resistivity
- Surface Resistivity per Square
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Resin Degradation Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|